DDA · Beam restoration · Updated November 2026

Beam Restoration and Repair Approval (DDA)

Beams show spalling at the soffit, rusted bottom bars and cracks long before they fail. Beam repairs need a repair design and, in DDA areas, DDA approval with the specialist stamp.

Beam damage shows first at the soffit: spalling, rust stains along the bottom bars and cracks. Cracks near the supports need an engineer before anything else. The repair design goes to DDA with the concrete restoration stamp.

TypicalCar park and basement beams
StampConcrete restoration
TestsBy a laboratory

Damage

Common beam damage

Car park and basement beams, balcony edge beams and beams below wet areas.

DamageCause or sign
Spalling at the soffitBottom bars exposed
Rusted bottom barsSection loss
Shear cracks near supportsNeed an engineer check
HoneycombingPoor original concreting

Investigation

What we investigate

A testing laboratory carries out the tests; our engineers choose the tests and read the results.

CheckHow
Crack patternBending, shear or corrosion
Bottom barsSection loss
Soffit concreteHollow areas mapped
SupportsBearing condition

Repair

How a beam repair is designed

The DDA route is on the concrete restoration stamp page.

PartNotes
ProppingBefore breaking out
Bar treatment or added barsWhere section is lost
Concrete repairRepair mortar or concrete
Strengthening if neededCFRP or steel after the repair

Official sites: DDA | Dubai Building Code

What you need to know

  • Cause first: bottom bars exposed.
  • Restoration stamp on the repair design.
  • Supervised repair works.
  • Needs more strength? See beam strengthening.

Documents you will need

  • Photos of the beam damage
  • Building details
  • Earlier reports, if any

How it works

Beam repair, step by step

1. Survey

Crack pattern.

2. Tests

Laboratory.

3. Design

Repair and method.

4. DDA

Stamp and approval.

5. Repair

Supervised.

Questions

Beam restoration questions

Do I need DDA approval to repair a beam?

Structural repairs do. We check your case and tell you if the repair is structural.

Are cracks in a beam always serious?

Not always. The pattern and width tell us; see crack assessment.

Is the restoration stamp different from the strengthening stamp?

It is the same strengthening specialist stamp. People call it the strengthening stamp, the concrete strengthening stamp, the concrete restoration stamp or the concrete repair stamp.

Related guides